{"id":92,"date":"2021-11-09T06:12:11","date_gmt":"2021-11-09T06:12:11","guid":{"rendered":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/?post_type=product&#038;p=92"},"modified":"2021-11-09T06:12:13","modified_gmt":"2021-11-09T06:12:13","slug":"noraa-block-board","status":"publish","type":"product","link":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/product\/noraa-block-board\/","title":{"rendered":"NORAA BLOCK BOARD"},"content":{"rendered":"<figure class=\"wp-block-table is-style-regular prop-table\">\n<table border=\"0\" width=\"100%\" cellspacing=\"2\" cellpadding=\"5\">\n<tbody>\n<tr>\n<td><strong>PROPERTY<\/strong><\/td>\n<td><strong>REQUIREMENT<\/strong><\/td>\n<td><strong>RESULT<\/strong><\/td>\n<\/tr>\n<tr>\n<td>Moisture content<\/td>\n<td valign=\"bottom\">5-15%<\/td>\n<td valign=\"bottom\">8-10%<\/td>\n<\/tr>\n<tr>\n<td>Change caused by humidity<\/td>\n<td valign=\"bottom\">Not more than \u00b11mm<\/td>\n<td valign=\"bottom\">Less than 0.6mm<\/td>\n<\/tr>\n<tr>\n<td>Adhesion of pliers<\/td>\n<td>excellent<\/td>\n<td>excellent<\/td>\n<\/tr>\n<tr>\n<td>Water resistant<\/td>\n<td>3hrs at 60\u00b0C \u00b12\u00b0C<br \/>\n72 hrs at 100\u00b0 C<\/td>\n<td>More than12 hrs at 60\u00b0 C<br \/>\nMore than72 hrs at100\u00b0 C<\/td>\n<\/tr>\n<tr>\n<td>Mycological test<\/td>\n<td>1 cycle of 21 days<\/td>\n<td>Can under go 3 cycles of 21days each without any edge separation.<\/td>\n<\/tr>\n<tr>\n<td>Modulus of rupture average<\/td>\n<td>40\/50 N\/mm^2<\/td>\n<td>45\/55 N\/mm^2<\/td>\n<\/tr>\n<tr>\n<td>Min individual<\/td>\n<td>34\/42N\/mm^2<\/td>\n<td>42\/48 N\/mm^2<\/td>\n<\/tr>\n<tr>\n<td>Modulus of Elasticity average<\/td>\n<td>4000\/5000 N\/mm^2<\/td>\n<td>4500\/5500 N\/mm^2<\/td>\n<\/tr>\n<tr>\n<td>Min individual<\/td>\n<td>3400\/4200N\/mm^2<\/td>\n<td>4500\/48 00N\/mm^2<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/figure>\n","protected":false},"excerpt":{"rendered":"<p>To ensure our commitment to quality Noraa block boards are made from top quality plantation timber logs, which are well seasoned and chemically treated before being converted into battens. The battens are then sandwiched between two mechanically dried veneers and then hot pressed. Noraa block boards are ideal for good strong support to specially wood work, because we believe that.<\/p>\n","protected":false},"featured_media":0,"comment_status":"open","ping_status":"closed","template":"","meta":[],"product_cat":[16],"product_tag":[],"_links":{"self":[{"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/product\/92"}],"collection":[{"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/product"}],"about":[{"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/comments?post=92"}],"wp:attachment":[{"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/media?parent=92"}],"wp:term":[{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/product_cat?post=92"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/demo.scorpiotechnologies.us\/noraa-ply\/wp-json\/wp\/v2\/product_tag?post=92"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}